Elevated temperature stability of carbon-fibre, nickel-matrix composites: morphological and mechanical property degradation

1973 ◽  
Vol 8 (2) ◽  
pp. 251-260 ◽  
Author(s):  
S. Sarian
2011 ◽  
Vol 261-263 ◽  
pp. 212-216
Author(s):  
Jun Lin Tao ◽  
Li Bo Qin ◽  
Kui Li ◽  
Bin Jia

Using micro-wave heating method, the previous disadvantages of heating slowly and non-uniform are broken through. And plain concrete high temperature loading experiment system is composed of the method and material experiment machine. Many experiments of self-made concrete are carried out from room temperature to 600°C by this system. The strength and critical strain of concrete with temperature are obtained, and through analysis of the compressive stress-strain curves under different temperature, the constitutive relationship is established. The result shows that this constitutive relationship is greatly agrees with experiment. Meanwhile, the phenomenon is analyzed and explained in the progress of experiment.


2012 ◽  
Vol 111 (10) ◽  
pp. 102808 ◽  
Author(s):  
Kin-Fu Kao ◽  
Yung-Ching Chu ◽  
Ming-Jinn Tsai ◽  
Tsung-Shune Chin

This paper presents the investigation of moderate properties of solidified Al (LM6)+SiCp metal matrix composite (AMMC). These AMMC is fabricated by considering five different parts of casting and different weight of SiCp for reinforcement. The SiCp wt. % is varied from 5 wt. % to 15 wt. % with a step size 5 %. During casting, temperature is measured using K-thermocouple and temperature vs. solidification curve is traced. These results are compared with the solidification results of Al (LM6) alloy. It is observed that the solidifying duration of AMMC increased as well as decreased liquid temperature by adding SiCp to it. The trend of the curve is also presented that the cooling rate and the duration of solidification are different for different part of casting. Mechanical property of the each five parts of casting is tabulated. It is observed from the properties that the mechanical properties of AMMC increased by increasing the wt. % of the reinforced particles SiCp.