porcelain glaze
Recently Published Documents


TOTAL DOCUMENTS

22
(FIVE YEARS 3)

H-INDEX

6
(FIVE YEARS 1)

Author(s):  
Camila Pauleski Zucuni ◽  
Gabriel Kalil Rocha Pereira ◽  
Kiara Serafini Dapieve ◽  
Marilia Pivetta Rippe ◽  
Marco Cícero Bottino ◽  
...  

2018 ◽  
Vol 19 (7) ◽  
pp. 589-598 ◽  
Author(s):  
Louisiane Verger ◽  
Olivier Dargaud ◽  
Gwenaëlle Rousse ◽  
Laurent Cormier
Keyword(s):  

2018 ◽  
Vol 32 (4) ◽  
pp. 174 ◽  
Author(s):  
Jean Soares Miranda ◽  
Natália Veloso Malta ◽  
Ronaldo Luís Almeida De Carvalho ◽  
Rodrigo Othávio de Assunção e Souza ◽  
João Paulo Barros Machado ◽  
...  

OBJECTIVE: to evaluated the influence of two types of low-fusing porcelain glaze application on the surface of a zirconia ceramics stabilized by yttrium (Y-TZP).METHODS: Y-TZP specimens were divided into five groups (n=5) according the surface treatments: control (CO), no treatment was performed; application of a thin low-fusing porcelain glass layer by the powder/liquid technique (GPL); GPL followed by 10% hydrofluoric acid (HF) etching (GPL-HF); glaze spray application (GS); GS followed by 10% HF etching (GS-HF). Roughness measurements contact angle, x-ray diffraction, energy-dispersive spectroscopy (EDS) and scanning electron microscope (SEM) analysis were performed.RESULTS: ANOVA and Tukey tests revealed that GPL had significantly lower contact angle values than the other groups (GPL:50.31º; GPL-HF: 72.73º; GS-HF: 81.73º; CO: 96.48º; GS:101.30º; p=0.001). GPL-HF presented a significant higher roughness (Ra/Rq: 2658.0/3367.0 ηm; p=0.001) than the other groups (GPL: 872.1/1162.0 ηm; GS-HF: 383.0/603.6 ηm; GS: 303.4/391.3 ηm; CO:263.4/339.1 ηm). The X-ray diffraction analysis just tetragonal phase in all groups. EDS and SEM analysis show a highest amount of silica on GPL and GPL-HF surface.CONCLUSION: the application of the low-fusing porcelain glaze by the powder/liquid technique followed by the HF etching promoted a better surface to micromechanical and chemical adhesion.


2017 ◽  
Vol 54 (2) ◽  
pp. 369-375
Author(s):  
Hale Yildizay ◽  
Hanife Kadioğlu
Keyword(s):  

2017 ◽  
Vol 43 (2) ◽  
pp. 1703-1709 ◽  
Author(s):  
Marcin Gajek ◽  
Janusz Partyka ◽  
Alicja Rapacz-Kmita ◽  
Katarzyna Gasek

2016 ◽  
Vol 27 (5) ◽  
pp. 543-547 ◽  
Author(s):  
Lígia Tiaki Yamamoto ◽  
◽  
Vinícius Anéas Rodrigues ◽  
Lucio Strazzabosco Dornelles ◽  
Marco Antonio Bottino ◽  
...  

Abstract The aim of this study was to assess whether surface treatment improves zirconia-porcelain adhesion. The 3Y-TZP blocks were cut into squares, then polished and sintered. The zirconia surface treatments were performed as follows: no treatment (C); tribochemical silica coating (TBS); glaze application + hydrofluoric acid etching (GA); glaze application + hydrofluoric acid etching + silanization (GAS); deposition of silica nanofilm (NF). After treatments, veneering porcelain cylinders (3.3 x 3.3 mm) were built up on all specimens and fired. Then the specimens were subjected to thermal cycling (6000 cycles), and subjected to shear test. Fractures were analyzed by stereomicroscopy and SEM. Data were statistically analyzed by 1-way ANOVA and Tukey's test (5%). Zirconia-porcelain bond strength was affected by the ceramic surface treatments (p=0.0001). GA (19.5±3 MPa) and GAS (16.2±4 MPa) recorded the highest bond strength values, while control group had the lowest bond value (10.1±4 MPa). Adhesive failure of the samples predominated. Therefore, glaze application as 3Y-TZP treatment before veneering porcelain stratification may enhance zirconia-porcelain adhesion.


2015 ◽  
Vol 41 (2) ◽  
pp. 2318-2327 ◽  
Author(s):  
Bruno Fabbri ◽  
Sabrina Gualtieri
Keyword(s):  

2015 ◽  
Vol 7 (12) ◽  
pp. 5034-5040 ◽  
Author(s):  
Zhian Bao ◽  
Honglin Yuan ◽  
Rui Wen ◽  
Kaiyun Chen

A fast and direct characterization of blue-and-white porcelain glaze from Jingdezhen is proposed using laser ablation-inductively coupled plasma mass spectrometry.